版权说明 操作指南
首页 > 成果 > 详情

硫酸肼还原浸出锌中浸渣中镉

认领
导出
Link by 中国知网学术期刊 Link by 万方学术期刊
反馈
分享
QQ微信 微博
成果类型:
期刊论文
论文标题(中文):
Reductive acid leaching of cadmium from zinc neutral leaching residue using hydrazine sulfate
作者:
Zhang, Chun;Min, Xiao-bo*;Zhang, Jian-qiang;Wang, Mi;Zhou, Bo-sheng;...
通讯作者:
Min, Xiao-bo
作者机构:
[Wang, Mi; Zhang, Chun; Shen, Chen; Min, Xiao-bo; Zhou, Bo-sheng; Zhang, Jian-qiang] Cent S Univ, Sch Met & Environm, Changsha 410083, Hunan, Peoples R China.
[Zhang, Chun] Hunan City Univ, Sch Municipal & Mapping Engn, Yiyang 413000, Peoples R China.
[Min, Xiao-bo] Cent S Univ, Chinese Natl Engn Res Ctr Control & Treatment Hea, Changsha 410083, Hunan, Peoples R China.
通讯机构:
[Min, Xiao-bo] C
Cent S Univ, Sch Met & Environm, Changsha 410083, Hunan, Peoples R China.
语种:
英文
关键词:
reductive acid leaching;zinc neutral leaching residue;hydrazine sulfate;cadmium
关键词(中文):
还原酸浸;锌中浸渣;硫酸肼;镉
期刊:
中国有色金属学报(英文版)
ISSN:
1003-6326
年:
2015
卷:
25
期:
12
页码:
4175-4182
基金类别:
Project(2012FJ1010)supported by the Key Project of Science and Technology of Hunan Province China Project(51474247)supported by the National Natural Science Foundation of China Project(2012GS430201)supported by the Science and Technology Program for Public Wellbeing China
机构署名:
本校为其他机构
院系归属:
市政与测绘工程学院
摘要:
Zinc neutral leaching residue (ZNLR) from hydrometallurgical zinc smelting processing can be determined as hazardous intermediate containing considerable amounts of Cd and Zn which have great threats to the environment. The ZNLR contained approximately 35.99% Zn, 15.93% Fe and 0.26% Cd, and Cd mainly existed as ferrites in the ZNLR in this research. Reductive acid leaching of ZNLR was investigated. The effects of hydrazine sulfate concentration, initial sulfuric acid concentration, temperature, duration and liquid-to-solid ratio on the extracti...
摘要(中文):
湿法炼锌中性浸出渣(中浸渣)是含有Cd和Zn等重金属元素的一种危险中间物料,对环境造成严重危害。本研究所用锌中浸渣含有约35.99%Zn、15.93%Fe和0.26%Cd,而Cd主要以铁酸盐的形式存在。研究硫酸肼浓度、硫酸初始浓度、温度、时间以及液固比对酸性还原浸出锌中浸渣Cd、Zn和Fe浸出率的影响。结果表明,中浸渣在硫酸肼浓度为33.3 g/L、硫酸初始浓度为80 g/L、浸出温度为95°C、液固比为10 m L/g、搅拌速度为400 r/min条件下还原浸出120 min,Cd、Zn和Fe的浸出率分别达90.81%、95.83%和94.19%。X射线衍射及扫描电镜-能谱分析显示还原浸出渣的主要物相为硫酸铅(Pb SO4)以及硫酸锌肼复盐((N2H5)2Z...