Simultaneous enhancement of strength and ductility in friction stir welded AZ31 alloy via multi-pass hot-rolling and subsequent annealing

认领
导出
Link by DOI
反馈
分享
QQ微信 微博
成果类型:
期刊论文
作者:
Wang, Qinghang;Zhai, Haowei;Chen, Shuai;Wang, Li;Huang, Lixin;...
通讯作者:
Hongbo Xia<&wdkj&>Yunwu Ma
作者机构:
[Wang, Qinghang; Wang, Li; Xia, Hongbo; Chen, Shuai; Zhai, Haowei] Yangzhou Univ, Sch Mech Engn, Yangzhou 225127, Peoples R China.
[Wang, Qinghang; Huang, Lixin] CIT Dicastal Co Ltd, Qinhuangdao 066000, Peoples R China.
[Zhao, Jun] Hunan City Univ, Sch Mech & Elect Engn, Yiyang 413002, Peoples R China.
[Ma, Yunwu] Shanghai Jiao Tong Univ, Sch Mech Engn, Shanghai Key Lab Digital Manufacture Thin Walled S, Shanghai 200240, Peoples R China.
[Ma, Yunwu] Shanghai Jiao Tong Univ, Sch Mech Engn, State Key Lab Mech Syst & Vibrat, Shanghai 200240, Peoples R China.
通讯机构:
[Hongbo Xia; Yunwu Ma] S
School of Mechanical Engineering, Yangzhou University, Yangzhou 225127, China<&wdkj&>Shanghai Key Laboratory of Digital Manufacture for Thin-walled Structures, School of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai 200240, China<&wdkj&>State Key Laboratory of Mechanical System and Vibration, School of Mechanical Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
语种:
英文
关键词:
AZ31 alloy;Friction stir welding;Multi-pass hot-rolling;Annealing;Mechanical properties
期刊:
Journal of Materials Research and Technology
ISSN:
2238-7854
年:
2023
卷:
23
页码:
5181-5192
基金类别:
National Natural Science Foundation of China [52204407, 52105405]; Natural Science Foundation of Jiangsu Province [BK20220595]; China Postdoctoral Science Foundation [2022M723689, 2021M702423]; Yangzhou University, China [YZ2020266]
机构署名:
本校为其他机构
院系归属:
机械与电气工程学院
摘要:
Friction stir welding (FSW) is a new solid-state joining process for joining light metals, such as magnesium (Mg) alloys. However, the texture-induced softening mechanism (in stir zone, SZ) tends to cause the worsening of mechanical properties in FSW Mg alloys. In this work, multi-pass hot-rolling and subsequent annealing is used to ameliorate the FSW AZ31 alloy plate. The results show that multi-pass hot-rolling leads to the c-axes of most grains in the SZ approximately perpendicular to the normal direction (ND) transforming into these almost parallel to the ND, accompanied with multiple twin...